Effect of zirconia addition on the microstructural evolution of porous hydroxyapatite
Resource
Ceramics International 33 (5): 715-718
Journal
Ceramics International
Journal Volume
33
Journal Issue
5
Pages
715-718
Date Issued
2007
Date
2007
Author(s)
Abstract
In the present study, 0-5 vol.% of 230 nm zirconia particles was added into hydroxyapatite (HAp). Though the reaction between HAp and ZrO2 has taken place, HAp remains after sintering at 1300 °C. The addition of zirconia reduces not only the sintering shrinkage, but also decreases the size of HAp grains. Both the strength and toughness of porous HAp decrease slightly due to the formation of CaZrO3 phase. © 2006 Elsevier Ltd and Techna Group S.r.l.