Abstract
Potassium niobate KNbO3 particles were synthesized via a newly developed glycothermal process using isopropanol as the reaction medium in supercritical environment. Increasing the concentration of KOH and the molar ratio of K+/Nb5+ substantially facilitated the formation of KNbO3. When the concentration was 0. 5 M and the molar ratio of K+/Nb5+ was greater than 2:1, well crystallized monophasic KNbO3 was successfully produced at as low as 250 °C. In comparison with the traditional hydrothermal process, the supercritical glycothermal process greatly reduced the required concentration of KOH. This supercritical glycothermal process provides a new prospective approach for synthesizing electronic ceramic powders at low temperatures. © 2002 Elsevier Science B.V. All rights reserved.
SDGs
Type
journal article
File(s)![Thumbnail Image]()
Loading...
Name
38.pdf
Size
225.37 KB
Format
Adobe PDF
Checksum
(MD5):b9500594d8011b1e9d3ba7da905db6cf