Magnetoresistance of la 0.7 Sr 0.3 MnO 3 film at room temperature
Journal
Journal of Magnetism and Magnetic Materials
Journal Volume
226-230
Journal Issue
PART I
Pages
690-692
Date Issued
2001
Author(s)
Abstract
The La0.7 Sr0.3MnO3 (LSMO) film is deposited successfully onto a MgO (001) substrate by using a magnetron DC sputtering system. The θ-20 X-ray diffraction pattern is detected to investigate the structure of the deposited LSMO film. According to the experimental temperature dependent magnetization result, the Curie temperature of the sample is 364.8 K. The magnetic hysteresis curve with a coercivity of 17 Oe was found for the LSMO film at 300K, meanwhile, a significant magnetoresistance was observed. With these properties at room temperature, the LSMO-based devices might be very suitable for practical applications. © 2001 Published by Elsevier Science B.V.
Subjects
Curie temperature; Magnetoresistance; Thin films- Ferromagnetic
Other Subjects
Curie temperature; Magnetoresistance; Magnetrons; Manganese oxide; X ray diffraction; DC sputtering; LSMO films; Magnetic hysteresis curves; Temperature-dependent magnetizations; Thin films-ferromagnetic; Thin films
Type