https://scholars.lib.ntu.edu.tw/handle/123456789/83227
DC 欄位 | 值 | 語言 |
---|---|---|
dc.contributor | 醫工所 | en |
dc.contributor.author | 林峰輝 | zh-tw |
dc.contributor.author | 洪敏雄 | zh-tw |
dc.contributor.author | 林繼昌 | zh-tw |
dc.contributor.author | 劉華昌 | zh-tw |
dc.contributor.author | 王正一 | zh-tw |
dc.contributor.author | LIN, FENG-HUEI | en |
dc.contributor.author | HON, MING-HSIUNG | en |
dc.contributor.author | LIN, CHI-CHANG | en |
dc.contributor.author | LIU, HWA-CHANG | en |
dc.contributor.author | WANG, CHENG-YI | en |
dc.creator | 林峰輝;洪敏雄;林繼昌;劉華昌;王正一 | - |
dc.creator | LIN, FENG-HUEI;HON, MING-HSIUNG;LIN, CHI-CHANG;LIU, HWA-CHANG;WANG, CHENG-YI | en |
dc.date | 1993 | en |
dc.date.accessioned | 2009-01-20T10:36:45Z | - |
dc.date.accessioned | 2018-06-29T00:51:25Z | - |
dc.date.available | 2009-01-20T10:36:45Z | - |
dc.date.available | 2018-06-29T00:51:25Z | - |
dc.date.issued | 1993 | - |
dc.identifier.uri | http://ntur.lib.ntu.edu.tw//handle/246246/105176 | - |
dc.description.abstract | The bioglass ceramics with chemical composition of NaO 8.4﹪, CaO 40.6﹪, SiO 39﹪ and PO 12﹪ showed a hgih bending strength and compressive strength and compressive strength of 160-190 MPa and 800-970 MPa Respectively. After nucleated at 800℃ for 50 minutes and crystalized at 890℃for 70 minutes, the specimen exhibited a fine and uniformed grain size of about 20 μm under optical microscopy. Biocompatibility test for the bioglass ceramics was conducted by the cell culture and implantcd in rat shoulder. The results showed that the specimens formed a tight chemical bond with biological texture and had a good biocompatibility.#A 3193116 | en |
dc.language | en-us | en |
dc.language.iso | en_US | - |
dc.relation | 中華醫學工程學刊 v.13 n.1 pp.31-45 | zh_TW |
dc.relation.ispartof | 中華醫學工程學刊,v.13 | - |
dc.subject | 生醫玻璃陶瓷 | en |
dc.subject | 結核 | en |
dc.subject | 結晶 | en |
dc.subject | 生物適應性 | en |
dc.subject | 貝它參鈣磷酸鹽 | en |
dc.subject | BIOGLASS CERAMICS | en |
dc.subject | NUCLEATION | en |
dc.subject | CRYSTALLIZATION | en |
dc.subject | BIOCOMPATIBILITY | en |
dc.subject | β- TRICALCIUMPHOSPHATE | en |
dc.title | Preparation and Characterization of High-Strength Bioglass Ceramics Composed of Na O-Cao-Sio -P O | en |
dc.title | 高強度鈉鈣矽磷生醫骨科玻璃陶瓷之研製 | zh_TW |
dc.relation.pages | 31-45 | - |
dc.relation.journalissue | n.1 | - |
item.fulltext | no fulltext | - |
item.languageiso639-1 | en_US | - |
item.grantfulltext | none | - |
crisitem.author.dept | Biomedical Engineering | - |
crisitem.author.dept | Biomedical Engineering | - |
crisitem.author.parentorg | College of Medicine | - |
crisitem.author.parentorg | College of Engineering | - |
crisitem.author.parentorg | College of Medicine | - |
crisitem.author.parentorg | College of Engineering | - |
顯示於: | 醫學工程學研究所 |
在 IR 系統中的文件,除了特別指名其著作權條款之外,均受到著作權保護,並且保留所有的權利。